Substandard Weather Resistance of Modified Acrylate-Epoxy-Phosphate-Distyrene Copolymer

Problem Phenomenon
The weather resistance of modified acrylate-epoxy-phosphate-distyrene copolymer is substandard, and after outdoor use, yellowing, embrittlement, or significant performance decline occurs
Cause Analysis
No ultraviolet absorber is added or the addition amount is insufficient The antioxidant system is imperfect The ultraviolet absorber has poor compatibility with the acrylate-epoxy-phosphate-distyrene copolymer The antioxidant is consumed and degraded during processing The formulation design is unreasonable
Solution
Add an appropriate amount of ultraviolet absorber (0.2-0.5%) Improve the antioxidant system with the combination of primary/secondary antioxidants Select a UV absorber with good compatibility Avoid high-temperature degradation of antioxidants during processing Optimize the formulation design
Key Takeaway
Weather resistance needs to be addressed from UV absorbers and antioxidants
weather resistanceultravioletantioxidantyellowing