Extrusion & Post
4 조회수
Uneven surface of styrene-acrylonitrile copolymer extruded profiles
문제 현상
The extruded profile surface is uneven, affecting product appearance and subsequent processing quality.
This problem is common in styrene-acrylonitrile copolymer extrusion production.
원인 분석
(1) Improper extrusion temperature (200-260°C) setting, with unstable melt quality
(2) Screw speed and haul-off speed are improperly matched
(3) Die condition or design problems
(4) Improper cooling system setting
(5) Raw material quality or pretreatment problems
해결 방법
(1) Optimize extrusion temperature to a reasonable value within the 200-260°C range
(2) Stabilize screw speed and haul-off speed
(3) Check die condition, clean material buildup or repair damage
(4) Adjust cooling water temperature and flow
(5) Ensure the raw material is dried (70-80°C, 3-4h) and clean
핵심 요약
Extrusion surface defects need to be controlled from three aspects: temperature, speed and die condition.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다