Extrusion & Post 3 Aufrufe

Uneven surface of styrene-acrylonitrile copolymer extruded profiles

Problembeschreibung
The extruded profile surface is uneven, affecting product appearance and subsequent processing quality. This problem is common in styrene-acrylonitrile copolymer extrusion production.
Ursachenanalyse
(1) Improper extrusion temperature (200-260°C) setting, with unstable melt quality (2) Screw speed and haul-off speed are improperly matched (3) Die condition or design problems (4) Improper cooling system setting (5) Raw material quality or pretreatment problems
Lösung
(1) Optimize extrusion temperature to a reasonable value within the 200-260°C range (2) Stabilize screw speed and haul-off speed (3) Check die condition, clean material buildup or repair damage (4) Adjust cooling water temperature and flow (5) Ensure the raw material is dried (70-80°C, 3-4h) and clean
Wichtigste Erkenntnis
Extrusion surface defects need to be controlled from three aspects: temperature, speed and die condition.