Molds & Tooling
3 views
Incomplete Purging / Color Change Contamination
Problem Phenomenon
Old color remains on the part after color change.
When this defect appears in parts of Process No.
1, it is usually related to specific process parameter ranges or equipment conditions.
If it persists, it will directly affect the part qualification rate and production cycle, increasing material loss and rework costs.
Timely diagnosis and elimination is a basic requirement for ensuring stable production.
Cause Analysis
1.
Mold design factors: residual material in the barrel, material accumulation in dead corners of the screw and check ring, carbon deposits inside the nozzle, hot runner residue.
2.
Temperature factors: the settings of barrel temperature and mold temperature directly affect melt fluidity, cooling rate, and crystallization behavior; low temperature is a common cause of filling and molding quality problems, and precise control is required according to the material's recommended processing window.
3.
Mold comprehensive factors: in addition to venting, mold design parameters such as cooling water channel layout, gate position and size, and demolding draft angle all have a systematic impact on part quality, and optimization is required from the source of mold design.
Solution
1.
Process parameter optimization and adjustment: use transition material to clean the barrel, disassemble and clean the screw and check ring, clean with special purging material, clean the hot runner system.
2.
Systematic troubleshooting method: troubleshoot item by item in the order of "parameters -> material -> mold -> equipment".
First adjust the parameters that are easiest to change, such as injection pressure and temperature, and observe the effect; if there is no improvement, check the drying and fluidity of the raw material; further check mold venting and gate design; finally check the mechanical condition of the equipment (check ring, screw).
Change only one variable at a time to determine the root cause.
3.
Preventive management: establish standardized process parameter cards and quality control limits for each mold/product, and regularly conduct process capability index (CPK) evaluation.
For recurring problems, use fishbone diagram or 5Why analysis to trace the root cause, and fix the countermeasures as PFMEA control points.
Key Takeaway
This problem is a typical manifestation of incomplete purging/color change contamination in '2079851475616104452; the core of the solution lies in eliminating the root cause of the defect through systematic optimization of process parameters (temperature, pressure, speed) and rationality checks of mold design.