Extrusion & Post
2 views
Uneven Distribution of Release Coating
Problem Phenomenon
The release force of the release paper/release film is uneven.
When this defect appears in coating-formed products, it is usually closely related to the coating head precision, the rheological properties of the coating liquid, the substrate surface condition, or the curing process conditions.
The distribution characteristics of coating defects (transverse/longitudinal/random) provide important clues for diagnosing coating head and curing system problems.
Continuous occurrence will cause the functional performance of the coating to fall below standard, and coordinated troubleshooting is required from three aspects: coating liquid formulation, coating equipment, and curing process.
Cause Analysis
1.
Comprehensive factor: uneven coating of the release agent (thickness fluctuation).
2.
Comprehensive factor: inconsistent curing degree of the release agent at different positions.
3.
Material/formulation factor: differences in substrate surface microstructure.
Solution
1.
Process parameter optimization and adjustment: use a high-precision coating method (such as five-roll coating).
2.
Mold/tooling improvement and maintenance: ensure the curing conditions (temperature, UV light intensity) are uniform across the web width.
3.
Equipment inspection and system maintenance: select a substrate with a uniform surface.
4.
Systematic troubleshooting method: troubleshooting of coating problems follows the sequence of "substrate → coating liquid → coating head → curing → environment".
First check the substrate surface tension (corona treatment effect) and cleanliness, then check the viscosity, solid content and degassing state of the coating liquid, next check the coating head gap and cleanliness, further verify the curing temperature and time, and finally evaluate the influence of ambient temperature, humidity and cleanliness.
5.
Preventive management: establish standardized process parameter cards and quality control limits for each mold/product, and regularly conduct process capability index (CPK) evaluations.
For recurring problems, use fishbone diagrams or the 5Why analysis method to trace the root cause, and solidify the countermeasures as PFMEA control points.
Establish a regular equipment maintenance system, and implement life management for key tooling such as dies/spinnerets/calender rolls/coating heads.
Key Takeaway
This problem is a typical manifestation of uneven distribution of release coating in coating forming.
The core of the solution lies in ensuring the substrate surface condition, optimizing the rheological properties of the coating liquid, and precisely controlling the curing process conditions.
It is recommended to start from the two aspects of substrate and coating liquid, and gradually troubleshoot to the coating equipment and curing system.