Extrusion & Post 1 views

HDPE extrusion sheet melt fracture

Problem Phenomenon
The HDPE sheet surface is periodically rough.
Cause Analysis
Exit shear exceeds the critical value; low die temperature and fast speed.
Solution
①Increase the die temperature; ②reduce speed; ③polish the die lip; ④add PPA processing aid.
Key Takeaway
Exit roughness = raise temperature, reduce speed, add aid.
HDPE; extrusion; melt fracture; die; PPA