Molds & Tooling 5 views

PA12 Product Flow Mark

Problem Phenomenon
Surface ripples.
Cause Analysis
Low front temperature; slow speed and small gate.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience; This mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solution
①Increase temperature; ②increase speed; ③enlarge gate; ④smooth filling.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes to facilitate locating effective measures
Key Takeaway
Flow marks are improved by temperature and speed.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a troubleshooting reference for subsequent similar problems
PA12;flow mark;temperature;speed;gate;filling