Material Drying 2 views

PA6 Toughened Grade Drying

Problem Phenomenon
Toughened PA6 injection molded after drying under conventional conditions still has slight silver streaks
Cause Analysis
Toughening modifiers (such as POE grafts) affect the diffusion rate of moisture in the particles, and toughened grades are more sensitive to moisture-induced hydrolysis, so conventional drying conditions have insufficient margin
Solution
Extend the drying time of toughened PA6 to 5-6 hours, and control the moisture content below 0.15%; preferentially select toughened grades with dry packaging and use immediately after opening
Key Takeaway
Toughened grades have higher hydrolysis sensitivity, and the drying standard must be raised accordingly; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
PA6toughenedhydrolysisdrying