Material Drying 5 views

PEI Hydrolysis Stability Verification

Problem Phenomenon
Performance tracking of PEI after boiling water or high-humidity environment applications; although hydrolytically stable, boundaries still need verification.
Cause Analysis
PEI has excellent hydrolysis stability, retaining 85% of tensile strength after 10000 hours of boiling water immersion; but long-term humidity and heat still accumulate; processing quality affects performance; application boundaries need data.
Solution
①Verify humidity-heat aging according to actual working conditions; ②processing quality ensures initial performance; ③collect long-term performance data; ④set application boundaries based on data.; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Key Takeaway
PEI hydrolysis stability is supported by ten-thousand-hour data; but boundary verification is still necessary; data accumulation optimizes applications.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PEI;hydrolysis;boiling water;humidity and heat;verification;boundary