Menu
Materials Machinery
Insights
Articles Videos Problem & Solution
About
About Chembull Media Partners
Contact Us
Language
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Back to Problem & Solution
Molds & Tooling 1 views

Improper PESU Mold Temperature

Problem Phenomenon
PESU products have high internal stress or poor surface quality; mold temperature deviates from the 149~163℃ range.
Cause Analysis
PESU mold temperature of 149~163℃ obtains low internal stress and high-performance products; low temperature means high stress and poor surface; high temperature means long cycle and mold sticking; uniformity affects consistency.
Solution
①Control mold temperature at 149~163℃; ②temperature uniformity management; ③balance stress and cycle; ④actually measure mold cavity temperature.; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Key Takeaway
The 149~163℃ of PESU mold temperature is the supplier standard; uniformity ensures consistency; balance optimization is based on verification.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PESU;mold temperature;149℃;stress;surface;uniformity

Was this helpful?

0 people found this helpful