Molds & Tooling 1 views

PESU Mold Design

Problem Phenomenon
PESU mold temperature 149~163℃ realization, heating and heat insulation.
Cause Analysis
PESU mold temperature 149~163℃; heating system capability; insulation plate; uniform temperature; cooling efficiency.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solution
①Heating system configuration; ②insulation plate use; ③uniform temperature; ④cooling optimization; ⑤actual measurement verification.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Key Takeaway
PESU high mold temperature is a process requirement; system design guarantees; actual measurement prevents deviation.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence