Material Drying 5 views

PET Sheet Extrusion Bubbles

Problem Phenomenon
Bubbles inside the sheet.
Cause Analysis
Water-containing hydrolysis produces gas; drying dew point not up to standard.
Solution
①Dehumidifying drying dew point ≤-40℃; ②check the drying system; ③vacuum check of the venting section.
Key Takeaway
Bubbles = drying dew point.
PET; sheet; bubble; drying; dew point

Was this helpful?