Material Drying 5 views

PET Preform Bubbles

Problem Phenomenon
Bubbles inside the preform body.
Cause Analysis
Water content (insufficient drying) or vacuum bubbles (insufficient holding pressure for thick walls).
Solution
①Verify drying; ②increase holding pressure; ③lower material temperature.
Key Takeaway
Bubbles = water or vacuum.
PET; preform; bubble; drying; holding pressure