Material Drying 1 views

PMMA Regrind Problems

Problem Phenomenon
Regrind parts have poor transparency and are brittle.
Cause Analysis
Regrind thermal history + moisture absorption; fine powder from crushed material.
Solution
①Ratio ≤20%; ②Re-dry; ③Optical parts prohibit regrind.
Key Takeaway
PMMA regrind = prohibited in transparent parts.