Processing Machinery 2 views

TPE Transparent Application

Problem Phenomenon
The transparency of transparent TPE products does not meet the standard
Cause Analysis
Transparent TPE has high requirements for formulation and process; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Solution
Select transparent-specific grades; precise process temperature; high-gloss mold; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Key Takeaway
Transparent TPE uses dedicated grades and precise processes; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
TPE transparency grade high gloss