Molds & Tooling 2 views

TPE flash

Problem Phenomenon
Flash at the parting line of TPE products
Cause Analysis
TPE has good fluidity and easily overflows; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Solution
Clamping calculation; pressure grading; parting line fitting; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Key Takeaway
For flash check clamping and grading; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
TPEflashclampingparting line