TPU Moisture Reabsorption Speed

Problem Phenomenon
Dried TPU was used after being placed in the workshop for 1 hour, and bubbles reappeared
Cause Analysis
TPU reabsorbs moisture extremely fast; dried material exposed to humid air reabsorbs excessive moisture within 30-60 minutes; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Solution
Dried material stored in an insulated drying hopper; usage time limited to within 30 minutes; re-dry if exceeded; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Key Takeaway
TPU dried material usage time limit is managed at 30 minutes; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future