Extrusion & Post 8 views

TPU Extrusion Temperature

Problem Phenomenon
TPU extrusion surface is wavy and the melt is unstable
Cause Analysis
Extrusion temperature fluctuation changes the melt viscosity; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting
Solution
Extrusion temperature stably controlled at 180-210°C; uniform die head temperature; melt pressure monitoring; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Key Takeaway
TPU extrusion temperature stability is the prerequisite for quality; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
TPUextrusion temperaturewavymelt pressure