Processing Machinery 3 views

TPU Film Yellowing

Problem Phenomenon
Transparent TPU film yellows after outdoor use
Cause Analysis
Aromatic TPU yellows under light exposure; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting
Solution
Choose aliphatic grades for outdoor transparent film; yellowing test verification; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Key Takeaway
Outdoor transparent film must be aliphatic; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future