Extrusion & Post 8 views

EEA extruded film has transverse ripples

Problem Phenomenon
Transverse periodic ripples on the EEA extruded film surface, wavelength 5-10mm
Cause Analysis
Haul-off roller vibration or unstable speed producing periodic stretching change; cooling roller eccentric or out-of-round surface causing periodic contact pressure change
Solution
1) Overhaul the haul-off roller to eliminate vibration; 2) Round the cooling roller, eccentricity <0.02mm; 3) Install a pressure stabilizing device on the extruder to eliminate pressure fluctuation; 4) Stable control of haul-off speed ±0.5%
Key Takeaway
Transverse ripples are caused by haul-off vibration and roller eccentricity; equipment overhaul and stable control are the key
EEA filmtransverse rippleshaul-off vibrationcooling roller eccentricitypressure stabilizing device