EMA Product Dimensional Change During Long-Term Storage

Problem Phenomenon
After 3 months of storage, EMA product dimensions change ±2-3%, exceeding the ±0.5% requirement
Cause Analysis
EMA physical aging relaxation causes continuous dimensional change; secondary crystallization slowly changes density and dimensions; low-molecular substances slowly migrate, changing local density
Solution
1) Anneal products at 80°C/4h before leaving the factory to stabilize dimensions; 2) Select high-molecular-weight grades to reduce low-molecular substances; 3) Slight crosslinking to reduce molecular chain mobility and inhibit aging; 4) Control storage environment temperature at 23±2°C to reduce the influence of temperature change
Key Takeaway
Dimensional change is caused by physical aging; annealing treatment and slight crosslinking are measures to stabilize dimensions
EMA dimensional stability physical aging annealing secondary crystallization slight crosslinking