Processing Machinery 2 views

Difficult EMA machine purging

Problem Phenomenon
EMA purging requires 2-3h, affecting changeover efficiency
Cause Analysis
EMA has strong adhesion forming a firm adhered layer on the screw and barrel; EMA has poor thermal stability and becomes sticky at high temperature, making it harder to remove
Solution
1) Flush with high-viscosity PE before purging to carry away EMA residue; 2) Lower purging temperature below EMA softening point to reduce adhesion; 3) Use dedicated purging compound
Key Takeaway
Difficult purging is caused by EMA's strong adhesion; PE flushing and temperature reduction are key
EMA difficult purging adhesion PE flushing dedicated purging compound