Processing Machinery 2 views

EMA internal unmelted particles

Problem Phenomenon
Unmelted transparent or translucent particles appear inside EMA products
Cause Analysis
Screw plasticizing capacity insufficient with temperature too low; feeding amount too large exceeding plasticizing capacity; EMA melting temperature too high
Solution
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase screw mixing section
Key Takeaway
Unmelted particles are caused by insufficient plasticization; increasing temperature and reducing feeding are key
EMA unmelted particles plasticizing capacity processing temperature screw mixing