EVA film blocking is severe
Problem Phenomenon
EVA film interlayer blocking >8N/15mm, cannot be slit
Cause Analysis
High VA content with strong surface adhesion; insufficient cooling, winding at >40°C
Solution
1) 0.3-0.5wt% erucamide antiblocking agent; 2) Winding <25°C; 3) 0.2wt% oleamide slip agent
Key Takeaway
EVA film blocking is caused by high VA tackiness and high-temperature winding; antiblocking agent and cooling are key