Material Drying 2 views

EVA foam cells are uneven

Problem Phenomenon
EVA foamed sheet cells 50-500μm, uneven in size
Cause Analysis
AC blowing agent unevenly dispersed, dry powder directly added; uneven melt viscosity
Solution
1) Blowing agent masterbatch method; 2) Fully mix EVA; 3) Crosslinking agent masterbatch method; 4) Mold ±2°C
Key Takeaway
Cell uniformity depends on blowing agent dispersion and crosslinking uniformity
EVA foam uneven cells blowing agent masterbatch crosslinking uniformity mold temperature control