Unmelted Particles Inside EVOH
Problem Phenomenon
Unmelted transparent or translucent particles appear inside EVOH products
Cause Analysis
Screw plasticizing capacity insufficient, temperature too low; feeding amount too large, exceeding plasticizing capacity; EVOH melting temperature too high
Solution
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase screw mixing section
Key Takeaway
Unmelted particles are caused by insufficient plasticizing; increasing temperature and reducing feeding are key