Material Analysis 9 views

Dimensional change of PVA products during long-term storage

Problem Phenomenon
After 3 months of storage, PVA product dimensions change ±2-3%, exceeding the ±0.5% requirement
Cause Analysis
PVA physical aging relaxation causes continuous dimensional change; secondary crystallization slowly changes density and dimensions; low molecular substances slowly migrate, changing local density
Solution
1) Anneal products at 80°C/4h before leaving the factory to stabilize dimensions; 2) Select high molecular weight grade to reduce low molecular substances; 3) Slight crosslinking to reduce molecular chain mobility and inhibit aging; 4) Control storage environment temperature at 23±2°C to reduce temperature change influence
Key Takeaway
Dimensional change is caused by physical aging; annealing treatment and slight crosslinking are measures to stabilize dimensions
PVA dimensional stability physical aging annealing secondary crystallization slight crosslinking