Material Drying 2 views

Tiger-skin-like stripes appear on the product surface

Problem Phenomenon
Tiger-skin-like stripes appear on the product surface, regular or irregular color bands alternately distributed, affecting appearance
Cause Analysis
Injection speed suddenly fast and slow, melt front unstable Mold temperature fluctuation Melt viscosity changes (temperature fluctuation or moisture change) Improper gate design produces unstable flow Holding pressure switchover too early
Solution
Stabilize injection speed, adopt multi-stage speed control Ensure the mold temperature is constant in the 40-80°C range Control barrel temperature and raw material moisture stable Optimize gate design, use fan gate Delay the holding pressure switchover timing
Key Takeaway
Tiger-skin stripes require stable injection parameters and mold temperature