Material Analysis
9 views
CMC Hardness Too High
Problem Phenomenon
Shore hardness of CMC products is 5-10 degrees higher than the target, feeling hard
Cause Analysis
CMC crystallinity is high and rigidity increases; too much filler added; cooling is too fast, crystallization is imperfect but rigidity is frozen in
Solution
1)Reduce cooling rate to perfect crystallization and reduce hard feel; 2)Reduce filler addition; 3)Add plasticizer 0.5wt% to reduce hardness
Key Takeaway
High hardness is caused by crystallization and filler; adjusting cooling and filler are the key
Was this helpful?
0 people found this helpful