Extrusion & Post 8 views

Glass Fibre extruded film winding wrinkling

Problem Phenomenon
Glass Fibre extruded film after winding shows transverse wrinkles and longitudinal creases
Cause Analysis
Film tension uneven, fluctuating ±20%; film thickness uneven causing inconsistent stretching of each section; shrinkage rate differs in each direction after cooling
Solution
1) Automatic tension control system to stabilize winding tension; 2) improve film thickness uniformity to ±5%; 3) adjust guide roller parallelism <0.05mm/m; 4) film fully cooled to <30°C before winding
Key Takeaway
Film wrinkling is caused by tension fluctuation and thickness unevenness; automatic tension control and uniformization are key
Glass Fibre filmwinding wrinklingtension controlthickness uniformityguide roller parallelism