Extrusion & Post 8 views

PB polybutene-1 slow crystallization problem in pipe extrusion

Problem Phenomenon
Polybutene-1 PB exhibits slow crystallization during pipe extrusion processing at 180-230°C.
Cause Analysis
PB molecular weight is the key factor.
Solution
Control cooling rate.
Key Takeaway
PB pressure pipes need to control crystal form transition.
PBpolybutene-1slow crystallizationpipe extrusioncrystal form transition