Extrusion & Post
8 views
PB polybutene-1 rough surface problem in pipe extrusion
Problem Phenomenon
Polybutene-1 PB exhibits rough surface during pipe extrusion processing at 180-230°C.
Cause Analysis
PB molecular weight is the key factor.
Solution
Optimize processing temperature.
Key Takeaway
PB pressure pipes need to control crystal form transition.
Was this helpful?
0 people found this helpful