The low peel strength problem of PBAK acrylate type in adhesive

Problem Phenomenon
Polybutyl acrylate-type PBAK exhibited low peel strength during adhesive processing at 80-150°C.
Cause Analysis
Improper drying conditions of PBAK caused the problem.
Solution
Improve the drying method.
Key Takeaway
PBAK for coating and adhesive applications requires fine formulation design.