Extrusion & Post 8 views

Optimization of the degradation problem of PBD in extrusion

Problem Phenomenon
Polybutadiene PBD, as an elastomer toughening modifier or HIPS component, exhibited degradation-related abnormalities during the extrusion process.
Cause Analysis
The Mooney viscosity of PBD affects processing; improper shear control leads to performance deterioration.
Solution
According to application requirements, optimize the compounding process to systematically solve the problem.
Key Takeaway
The core of PBD processing lies in thermal-oxidative protection.
PBDpolybutadieneHIPS