Material Analysis
9 views
PBD shear rate Regulation and Processing Stability
Problem Phenomenon
PBD exhibits shear rate-related process abnormalities in open milling.
Cause Analysis
Under the PBD processing temperature of 140-180°C, improper setting of the shear rate parameters leads to Mooney viscosity drift.
Solution
Optimize the shear rate and add antioxidant 2246.
Key Takeaway
In PBD processing, shear rate control is the foundation of quality stability.