Molds & Tooling
2 views
PBN mold carbon buildup Problem in Sheet Processing
Problem Phenomenon
Polybutylene naphthalate PBN exhibits mold carbon buildup in sheet processing at 270-300°C.
Cause Analysis
Under high-temperature processing at 270-300°C, degradation causes the problem.
Solution
Solve by drying to a moisture content of <50ppm.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.
Was this helpful?