Extrusion & Post 8 views

PBN flow mark Problem in Drawing Processing

Problem Phenomenon
Polybutylene naphthalate PBN exhibits flow mark in drawing processing at 270-300°C.
Cause Analysis
Under high-temperature processing at 270-300°C, crystallization causes the problem.
Solution
Solve by drying to a moisture content of <50ppm.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.
PBNflow markhigh temperaturedrawingprotection