PBN viscosity decrease problem in film processing
Problem Phenomenon
Polybutylene naphthalate PBN shows viscosity decrease in film processing at 270-300°C.
Cause Analysis
Crystallization under high-temperature processing at 270-300°C triggers the problem.
Solution
Solved by nitrogen protection.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.