Material Drying 2 views

Low crystallinity problem of PBS biodegradable material in injection

Problem Phenomenon
Polybutylene succinate PBS shows low crystallinity in injection processing at 140-200°C.
Cause Analysis
Caused by poor thermal stability of PBS and moisture sensitivity.
Solution
Improved by adding an anti-hydrolysis agent.
Key Takeaway
The degradation characteristics of PBS require gentle processing.