Material Drying 2 views

PBS biodegradable material bubbles problem in spinning

Problem Phenomenon
Polybutylene succinate (PBS) exhibits bubbles during spinning processing at 140-200°C.
Cause Analysis
Caused by poor thermal stability and moisture sensitivity of PBS.
Solution
Improve by lowering the processing temperature.
Key Takeaway
The degradation characteristics of PBS require mild processing.
PBSbiodegradationbubblesspinningthermal stability