Extrusion & Post 8 views

Solution for demolding effect of calcium-zinc stabilizer in powder coating

Problem Phenomenon
The calcium-zinc PVC system shows demolding effect-related abnormalities in the powder coating production stage, customers complain.
Cause Analysis
The initial coloring characteristic of calcium-zinc stabilizers produces demolding effect problems under specific working conditions.
Solution
From the formulation perspective, increase auxiliary stabilizers, combined with process optimization to solve it.
Key Takeaway
The demolding effect problem of the calcium-zinc system in the powder coating stage requires bidirectional adjustment of formulation and process.