Material Drying
2 views
Control of viscosity abnormality in PEOX '2079851475616104458 water-soluble bags
Problem Phenomenon
During PEOX '2079851475616104458 production of water-soluble bags, the problem of not up to standard viscosity occurs.
Cause Analysis
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.3% exceeding the standard, and insufficient cooling.
Solution
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Key Takeaway
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.