Material Drying
2 views
Control of appearance abnormality in PEOX hot pressing agricultural products
Problem Phenomenon
During PEOX hot pressing production of agricultural products, the problem of uneven appearance occurs.
Cause Analysis
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.3% exceeding the standard, and shear heat accumulation.
Solution
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Key Takeaway
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.