Material Drying
2 views
Control of viscosity abnormality in PEOX hot pressing medical products
Problem Phenomenon
During PEOX hot pressing production of medical products, the problem of large fluctuation in viscosity occurs.
Cause Analysis
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
Solution
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and strengthen cooling.
Key Takeaway
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
Was this helpful?
0 people found this helpful