Material Analysis 2 views

Regulation of dispersion white spots of PPA in cast CPP Processing

Problem Phenomenon
The dispersion white spots abnormality of the PPA processing aid in cast CPP production affects output.
Cause Analysis
The dispersion white spots of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.02%, and the molecular weight needs to be optimized.
Solution
Adjust the PPA addition amount combined with screw design.
Key Takeaway
The key to the performance of PPA lies in matching with the base resin.
PPAcast CPPdispersion white spotsfluoropolymerprocessing aid