Material Analysis 2 views

Processing difficulty with high filler loading

Problem Phenomenon
After filler >100 parts, flowability is extremely poor
Cause Analysis
Filler increases viscosity, large surface area
Solution
Reduce filler, add processing oil
Key Takeaway
High loading is a cost strategy