Back to Problem & Solution
Extrusion & Post 2 views

POE film blocking, difficult delamination

Problem Phenomenon
POE film interlayer blocking, delamination force >5N/15mm, automatic slitting machine cannot delaminate
Cause Analysis
POE surface adhesion is strong; film temperature too high >40°C during winding; low molecular substances migrate to the surface forming an adhesive layer
Solution
1) Add 0.3-0.5wt% antiblocking agent erucamide; 2) Fully cool to <25°C before winding; 3) Add 0.2wt% slip agent to synergistically reduce blocking; 4) Reduce winding tension to decrease interlayer pressure
Key Takeaway
Film blocking is caused by surface tackiness and high-temperature winding; antiblocking agent and full cooling are effective countermeasures