Extrusion & Post 4 views

POE surface snakeskin pattern

Problem Phenomenon
POE extruded product surface snakeskin-like irregular texture
Cause Analysis
Extrusion temperature too low, melt elastic recovery uneven; die temperature distribution uneven
Solution
1) Raise extrusion temperature to the processing temperature range; 2) Die temperature uniformized ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Key Takeaway
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are key
POEsnakeskin patternextrusion temperatureelastic recoverydie temperature control