Extrusion & Post
1 views
Insufficient peel strength of coating layer
Problem Phenomenon
Low peel strength after coating is composited with metal
Cause Analysis
Insufficient sandblasting roughness and insufficient bonding layer temperature
Solution
Sa2.5 sandblasting Rz50-80, MAH grafted primer 260-280C
Key Takeaway
Peel strength involves multi-factor synergy
Was this helpful?
0 people found this helpful