Extrusion & Post 1 views

Coating orange peel defect

Problem Phenomenon
Electrostatic sprayed coating has orange peel and low gloss
Cause Analysis
Powder particle size too coarse, wide distribution, slow heating rate
Solution
Control D50 at 35-50um, rapidly heat to 240-260C
Key Takeaway
Leveling directly affects anti-corrosion life